Quality & Certificate of Interlocking Rubber tiles

We, being a quality conscious organization, make it a point to implement and adhere to stringent and rigorous quality control measures that are at par with the international standards in the manufacturing process.

This helps us in maintaining the quality standards of our products.

Our products are tested by ASTM standards and EN standards.

Test method Test Value Tested laboratory name
ASTM D2859 Pill flammability Excellent pass TSI Georgia USA
ASTM E303-93 Skid Resistance Excellent pass TSI Georgia USA
ASTM D2240 Hardness Shore A59 TUV Rheinland INDIA
ASTM F 150 Ground Electrical Resistance M ohms 168 TUV Rheinland INDIA
DIN 53577 Compression Strength Test Thickness = 42mm Load= 19950.83 N Compression Strength at 25% deflection = 4.39Mpa TUV Rheinland INDIA
ASTM D573/ASTM D412 Tensile Properties(After Aging at 70oC for 72 hrs)Tensile Strength MPA 1.01 TUV Rheinland INDIA
FMVSS 302 Burning Behaviour Test 6.8 mm/min TUV Rheinland INDIA
ASTM G21:2015 Aspergillus nigerATCC16404 Penicillium pinophilum Hedgcock ATCC 9644 Chaetomium glososum ATCC 6205 Trichoderma virens ATCC 9645 Aureobasidium pullulans ATCC 15233 Observed Growth on Specimen None TUV Rheinland INDIA
ASTM C 423 Sound Absorption Coefficients 0.45 Noise Reduction Coefficient (NRC) TUV Rheinland INDIA
AS/ISO 9239.1-2003 Reaction to Fire Tests for Floorings. Determination of the Burning Behaviour using a Radiant Heat Source CHF Value 1 Non Directional ≤1.1 kW/m² Smoke Value 1 Non Directional 1869 %.min Australian Wool Testing Authority Ltd - trading as AWTA Product Testing
UV Exposure (150*C) By chemical Analysis ISO: 4 SBR Blend Rubber No effect Alekh Plastic Testing Centres

Note: we can give you all physical soft copy by email with customer genuine requirement.